Secant Modulus, MD 0.228 GPa
33.1 ksi
1% Strain; ASTM D882
M. Holland Company LL104 LLDPE  (discontinued **)
Additives: Antiblock, SlipFeatures: Unspecified Antiblocking, Butene Comonomer, Copolymer, Good Drawdown, Good Processability, Unspecified SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c) 2.2..
Secant Modulus, MD 0.228 GPa
33.1 ksi
Film value
Dow Elite® 5110 Linear Low Density Polyethylene
5110 enhanced polyethylene resin is a copolymer produced via INSITE Technology from Dow Plastics. It offers unique combination of high modulus and excellent impact strength, allowing for downgaugin..