Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.241 GPa | 35.0 ksi | ASTM D882 |
ExxonMobil Escorene® LL-3105 LLDPE/Hexene Premium Film Resin, Tough
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3105 have outstanding tensile and toughness properties. The superior strength propert.. |