Polymer Property : Secant Modulus, MD = 0.278 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.278 GPa
40.3 ksi
1%; ASTM D882
Braskem LQ 0518/21 AF LLDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Coextruded film for automatic packaging (FFS). Information provided by Braskem