Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.310 GPa | 45.0 ksi | ASTM D882-A |
Borealis Himod™ FT7324 . LDPE for Film Himod FT7324 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Secant Modulus, MD | 0.310 GPa | 45.0 ksi | ASTM D882 |
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 1.2 mil Film, Stiff
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |