Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.750 GPa | 109 ksi | ASTM D882 |
Chevron Phillips HiD® 9606 HDPE Blown Film and Sheet
(discontinued **) Resin Type: ASTM D 4976 Classification: PE 235, A 54502Applications:General Purpose Films and Sheet, Coextruded Film Structures, Deli and Tissue Films, Sheet Thermoforming Applications with Good Str.. |
|||
Secant Modulus, MD | 0.750 GPa | 109 ksi | ISO 527-3 |
Borealis Borclear™ RB707CF Polypropylene Random Copolymer for Blown Film Borclear RB707CF is a propylene-ethylene copolymer film resin without slip and antiblock additives, suitable for the manufacturing of unoriented film on blown film process.Borclear RB707CF is especi.. |