Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.179 - 1.05 GPa | 26.0 - 152 ksi | Average value: 0.427 GPa Grade Count:13 |
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m.. |