Polymer Property : Secant Modulus, MD = 1.31 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 1.034 - 1.31 GPa
150.0 - 190 ksi
ASTM D882
Honeywell ACLAR® 11A (3.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Secant Modulus, MD 1.034 - 1.31 GPa
150.0 - 190 ksi
ASTM D882
Honeywell ACLAR® 11A (2.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.