Polymer Property : Secant Modulus, MD = 1.517 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 1.517 - 1.793 GPa
220.0 - 260.1 ksi
ASTM D882
Honeywell ACLAR® 33C (0.75 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell..