Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 1.338 - 1.53 GPa | 194.1 - 222 ksi | ASTM D882 |
Honeywell ETFE EX30 Mono-Axially Oriented, ETFE Film
(discontinued **) Description: ETFE EX30 is a 1.2 mil (30 micron) mono-axially oriented, ethylene tetrafluoroethylene (ETFE) film. It offers superior weather ability, UV transmission, chemical and graffiti resistanc.. |