Secant Modulus, MD 1.724 - 2.586 GPa
250.0 - 375.1 ksi
ASTM D882
Honeywell Capran® Oxyshield™ M-OPA (0.60 mil) Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film
Description: Capran® Oxyshield™ M-OPA (Machine Direction Oriented Polyamide) is a clear, monoaxially oriented, co-extruded in-line nylon6/nylon6/nylon6 film with high mechanical strength and..
Secant Modulus, MD 1.724 - 2.586 GPa
250.0 - 375.1 ksi
ASTM D882
Honeywell Capran® Oxyshield™ M-OPA (0.75 mil) Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film
Description: Capran® Oxyshield™ M-OPA (Machine Direction Oriented Polyamide) is a clear, monoaxially oriented, co-extruded in-line nylon6/nylon6/nylon6 film with high mechanical strength and..
Secant Modulus, MD 1.724 - 2.586 GPa
250.0 - 375.1 ksi
ASTM D882
Honeywell Capran® Oxyshield™ M-OPA (1.0 mil) Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film
Description: Capran® Oxyshield™ M-OPA (Machine Direction Oriented Polyamide) is a clear, monoaxially oriented, co-extruded in-line nylon6/nylon6/nylon6 film with high mechanical strength and..