Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 1.765 GPa | 256.0 ksi | 300°C; ASTM D882 |
UBE UPILEX VT Polyimide Film Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries.. |