Polymer Property : Secant Modulus, MD = 23.9 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.165 GPa
23.9 ksi
ASTM D882
NOVA Chemicals Novapol® LF-0323-A LDPE Film Resin
Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Food wrap, consumer packaging, liners, blends with LLDPE.Data provid..
Secant Modulus, MD 0.165 GPa
23.9 ksi
ASTM D882
NOVA Chemicals Novapol® LF-0323-B LDPE Film Resin
Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Bakery bags, sandwich bags, zipper lock bags, cast film.Data provide..
Secant Modulus, MD 0.165 GPa
23.9 ksi
50 µm (2 mil) film; ASTM D882
DuPont Nucrel® 1202HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
11.5 wt% Methacrylic Acid.Nucrel® 1202HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment des..
Secant Modulus, MD 0.165 GPa
23.9 ksi
ASTM D882
Chevron Phillips MarFlex® 5628 LDPE Blown Film Resin
Resin Type: HomopolymerCharacteristics: Superior tensile and impact strengthGood abrasion and tear resistanceExcellent retention of properties after agingApplications: LaminationsPallet shrinkcase s..
Secant Modulus, MD 0.165 GPa
23.9 ksi
at 1%; ASTM D882
NOVA Chemicals Sclair® 11C1 Octene LLDPE Film Resin  (discontinued **)
Low gel, Good processability, Excellent mechanical propertiesApplications: Shrink filmAdditives: Process stabilizerFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but ..