Secant Modulus, MD 0.166 GPa
24.1 ksi
ASTM D882
Huntsman PE 1017 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, Drug Master File listed product, and FDA compliant.Features: Good impact strength, good machinability, heat seal and foaming characteristicsApplications: Film Extrusion: industrial line..
Secant Modulus, MD 0.166 GPa
24.1 ksi
ASTM D882
Huntsman PE1023 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Good draw down characteristics.Applications: Film extrusion: drum liners, hardware packaging, and refuse bags.FDA Notes: Conforms to FDA regulation 21 CFR 17..
Secant Modulus, MD 0.166 GPa
24.1 ksi
ASTM D882
Huntsman PE1201 EVA Film Extrusion  (discontinued **)
2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Good optical, medium impact strength, and good processability.Applications: Film extrusion: heavy duty packaging.FDA Notes: Conforms to FDA ..