Polymer Property : Secant Modulus, MD = 240 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.448 - 1.65 GPa
65.0 - 240 ksi
Average value: 1.21 GPa Grade Count:15
Overview of materials for Polychlorotrifluoroethylene; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu..