Polymer Property : Secant Modulus, MD = 25.8 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.178 GPa
25.8 ksi
1%; ASTM D882
Braskem LL 118/21 LLDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem