Mechanical Properties Metric English Comments
Secant Modulus, MD 0.152 - 0.208 GPa
22.0 - 30.2 ksi
Average value: 0.177 GPa Grade Count:4
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum ..