Mechanical Properties Metric English Comments
Secant Modulus, MD 0.221 GPa
32.1 ksi
ASTM D882
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a..
Secant Modulus, MD 0.221 GPa
32.1 ksi
ASTM D882
Huntsman PE1033 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Good opticals, impact strength, good processing properties, and stiffnessApplications: Film extrusion: general purpose packaging and film applications.FDA No..
Secant Modulus, MD 0.221 GPa
32.1 ksi
ASTM D882
Huntsman PE1065 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Yields film with excellent optical and machinability.Applications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms to FDA regu..
Secant Modulus, MD 0.221 GPa
32.1 ksi
1% Strain; ASTM D882
M. Holland Company LD225 LDPE  (discontinued **)
Additives: Medium Antiblock, Medium SlipFeatures: Medium Antiblocking, High Clarity, High Gloss, Heat Sealable, Good Processability, Medium SlipUses: FilmProcessing Method: Blown FilmInformation pro..