Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 3.30 GPa | 479 ksi | ASTM D882 |
NatureWorks® Ingeo™ 4043D General Purpose Film Grade Biopolymer Ingeo 4043D can be converted into a biaxially oriented film with use temperatures up to 265ºF (130ºC). This film has excellent optics, good machinability and excellent twist and deadfold. These pr.. |