Polymer Property : Secant Modulus, MD = 5.42 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.0374 - 0.117 GPa
5.42 - 17.0 ksi
Average value: 0.0727 GPa Grade Count:9
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Film Grade". Each property range of values reported is minimum a..