Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 1.76 - 9.12 GPa | 256 - 1320 ksi | Average value: 5.34 GPa Grade Count:3 |
Overview of materials for Polyimide, Thermoset Film This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr.. |