Mechanical Properties Metric English Comments
Secant Modulus, TD 0.00145 - 0.869 GPa
0.210 - 126 ksi
Average value: 0.222 GPa Grade Count:194
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum ..