Polymer Property : Secant Modulus, TD = 0.0620 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.0620 GPa
8.99 ksi
ASTM D882
ExxonMobil Escorene® LD-734 High EVA Extrusion Coating Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and..