Secant Modulus, TD 0.0712 GPa
10.3 ksi
Film value
Dow AFFINITY™ PL 1850 Polyolefin Plastomer
AFFINITY® PL 1850 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide blown and cast film products with low temperature sealability, excellent optics and good abuse resistanc..