Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.112 GPa | 16.2 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trilene® TS 8058 LLDPE-C6 and LDPE Blend The Trilene TS 8058 product is a blend with a high ratio of linear low-density polyethylene - hexene comonomer (LLDPE-C6) with low-density polyethylene (LDPE) excellent mechanical resistance, along .. |