Mechanical Properties Metric English Comments
Secant Modulus, TD 0.125 GPa
18.1 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film
The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng..
Secant Modulus, TD 0.125 GPa
18.1 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TS 7003 LDPE - High Strength Film
The Trithene TS 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily proc..
Secant Modulus, TD 0.125 GPa
18.1 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film
The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength..
Secant Modulus, TD 0.125 GPa
18.1 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TX 7003 LDPE - Heavy Duty and Industrial Film
The Trithene® TX 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and environmental stress cracking resistance (ESCR). Additionally, this product..