Secant Modulus, TD 0.137 GPa
19.9 ksi
ASTM D882
ExxonMobil Exceed™ 357C32 LDPE/Hexene Premium Cast Stretch Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 357C32 resin have outstanding tensile properties and..