Polymer Property : Secant Modulus, TD = 0.1755 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.1755 GPa
25.45 ksi
2% Secant; ASTM D882
Dow ELITE™ 5500G Enhanced Polyethylene Resin
™ 5500G is a copolymer produced via INSITE™ Technology. It offers an exceptional combination of processability, low heat seal initiation temperature, package integrity, optical properties, and te..