Polymer Property : Secant Modulus, TD = 0.3485 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.3485 GPa
50.54 ksi
2% Secant; ASTM D882
Dow DOWLEX™ 2038.68G Linear Low Density Polyethylene
Fast processing on narrow die gaps For blown film paper product over wrap applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow