Mechanical Properties Metric English Comments
Secant Modulus, TD 0.360 GPa
52.2 ksi
ASTM D882-A
Borealis Himodâ„¢ FT7324 . LDPE for Film
Himod FT7324 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..