Mechanical Properties Metric English Comments
Secant Modulus, TD 0.410 GPa
59.5 ksi
ASTM D882
NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin
Film Properties. Features: Excellent stiffness, excellent puncture, high strength and toughness.Applications: Industrial packaging, overwrap, narrow die gap extrusion.Data provided by the manufactu..