Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.958 GPa | 139 ksi | ASTM D882 |
LyondellBasell Alathon® L5005V High Density Polyethylene, HMW Film Grade ALATHON L5005V is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typical applicati.. |