Polymer Property : Secant Modulus, TD = 1.448 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 1.138 - 1.448 GPa
165.1 - 210.0 ksi
ASTM D882
Honeywell ACLAR® SupRx 900 CTFE Homopolymer, Barrier Film
Description: ACLAR® SupRx 900 is a .9 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme..