Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.765 - 0.830 GPa | 111 - 120 ksi | ASTM D882 |
Honeywell ETFE EX30 Mono-Axially Oriented, ETFE Film
(discontinued **) Description: ETFE EX30 is a 1.2 mil (30 micron) mono-axially oriented, ethylene tetrafluoroethylene (ETFE) film. It offers superior weather ability, UV transmission, chemical and graffiti resistanc.. |