Secant Modulus, TD 1.07 GPa
155 ksi
ASTM D882
LyondellBasell Alathon® H6012 High Density Polyethylene, MMW Film Grade
ALATHON H6012 is medium molecular weight high density polyethylene homopolymer for use in cast film applications. Typical applications for this resin include extrusion coating, blends with LDPE and ..
Copyright © lookpolymers.com All Rights Reserved