Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.120 GPa
17.4 ksi
ASTM D882
Eastman 5265 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Excellent heat seal characteristics, Good optical properties, Superior impact strength, Low coefficient of friction, Good processability, High Slip, High Ant..
Secant Modulus, TD 0.120 GPa
17.4 ksi
ASTM D882
Eastman 5267 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Excellent heat seal characteristics, Excellent impact strength, Good optical properties, Good processability, High antiblock, No slipApplications:Laminations..
Secant Modulus, TD 0.120 GPa
17.4 ksi
ASTM D882
Eastman 5269 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin  (discontinued **)
Resin Type: CopolymerCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flow for Injection Blow Molding Applications, Good Par..
Secant Modulus, TD 0.120 GPa
17.4 ksi
ASTM D882
Eastman 5282 LDPE 8% EVA Copolymer, High Clarity, High Impact Film Resin  (discontinued **)
Resin Type: CopolymerCharacteristics: Excellent Heat Seal Characteristics, Superior Impact Strength, Good Optical Properties, Low Slip, High Antiblock, Good Bubble Stability at High Draw Down Speeds..
Secant Modulus, TD 0.120 GPa
17.4 ksi
ASTM D882
Eastman 5284 LDPE 8% EVA Copolymer, High Clarity, Ultra-High Impact Film Resin  (discontinued **)
Resin Type: CopolymerCharacteristics: Excellent Heat Seal Characteristics, Superior Impact Strength, Good Optical Properties, No Slip, High Antiblock, High Coefficient of FrictionApplications:Ice Ba..