Mechanical Properties Metric English Comments
Secant Modulus, TD 0.862 - 1.207 GPa
125 - 175.1 ksi
ASTM D882
Honeywell ACLAR® 22C (10.0 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe..
Secant Modulus, TD 0.862 - 1.207 GPa
125 - 175.1 ksi
ASTM D882
Honeywell ACLAR® 22C (7.50 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe..
Secant Modulus, TD 0.862 - 1.207 GPa
125 - 175.1 ksi
ASTM D882
Honeywell ACLAR® 22C (3.00 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe..