Polymer Property : Secant Modulus, TD = 218 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 1.50 GPa
218 ksi
ASTM D882
Honeywell Oxyshieldâ„¢ BOEB Biaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film
Description: Oxyshieldâ„¢ BOEB is a 0.60 mil (15 micron) biaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of relative humidity. T..
Secant Modulus, TD 1.50 GPa
218 ksi
ASTM D882
Solvay Specialty Polymers Ajedium™ Films -- Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Halar® ECTFE is a semi-crystalline fluoropolymer with a chemical structure of a 1:1 alternating copolymer of ethylene and chlorotrifluoroethylene.Halar® film is a strong, hard, tough, abrasion..