Polymer Property : Secant Modulus, TD = 22.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.152 GPa
22.0 ksi
ASTM D882
Huntsman Rexell® V8801 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and..
Secant Modulus, TD 0.152 GPa
22.0 ksi
ASTM D882
Huntsman PE1407 EVA Film Extrusion  (discontinued **)
4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Secant Modulus, TD 0.152 GPa
22.0 ksi
50 µm (2 mil) film; ASTM D882
DuPont Nucrel® 1202HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
11.5 wt% Methacrylic Acid.Nucrel® 1202HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment des..
Secant Modulus, TD 0.152 GPa
22.0 ksi
ASTM D882
Huntsman Rexell® V8403 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and..
Secant Modulus, TD 0.152 - 0.276 GPa
22.0 - 40.0 ksi
Average value: 0.218 GPa Grade Count:12
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..