Mechanical Properties Metric English Comments
Secant Modulus, TD 0.159 GPa
23.1 ksi
ASTM D882
ExxonMobil Escorene® LL-3023 LLDPE/Hexene Premium Cast Stretch Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3023 have outstanding tensile properties as well as stiffness and toughness.Applicatio..
Secant Modulus, TD 0.159 GPa
23.1 ksi
2% Secant; ASTM D882
Dow DAF 780 Carpet Underlayment Adhesion Film
DAF 780 is a low melt point, coextruded film used to improve slip characteristics of polyurethane foam for carpet installation or other applications.Information provided by Dow
Secant Modulus, TD 0.159 GPa
23.1 ksi
ASTM D882
ExxonMobil Escorene® LL-3003 LLDPE/Hexene Premium Cast Stretch Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3003 have outstanding tensile properties as well as stiffness and toughness.Applicatio..
Secant Modulus, TD 0.159 GPa
23.1 ksi
ASTM D882
Huntsman Rexell® L8102 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer with high slip and medium antiblock, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.A..
Secant Modulus, TD 0.159 GPa
23.1 ksi
ASTM D882
Huntsman PE1403 EVA Film Extrusion  (discontinued **)
4% Vinyl Acetate EVA Copolymer, DMF listed and FDA compliantFeatures: High clarity film with good toughness and flexibility at low temperatures.Applications: Film extrusion: frozen food and general ..