Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.175 GPa | 25.4 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® LA-0219-AM LDPE Foam Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blo.. |
|||
Secant Modulus, TD | 0.175 GPa | 25.4 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® LF-0219-A LDPE Film Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinInformation provided by NOVA Chemi.. |
|||
Secant Modulus, TD | 0.175 GPa | 25.4 ksi | ASTM D882 |
NOVA Chemicals Novapol® LF-0219-D LDPE Film Resin Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Liners, industrial packaging, blends with LLDPE.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.175 GPa | 25.4 ksi | 50 µm (2 mil) film; ASTM D882 |
DuPont Nucrel® 30707SR Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
(discontinued **) 7 wt% Acrylic Acid.Nucrel® 30707SR is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusio.. |
|||
Secant Modulus, TD | 0.175 GPa | 25.4 ksi | ASTM D882 |
NOVA Chemicals Novapol® LF-0218-AB LDPE Film Resin
(discontinued **) Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu.. |
|||
Secant Modulus, TD | 0.175 GPa | 25.4 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® LA-0218-AB LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Good heat sealing latitude, Moderate toughness, E.. |
|||
Secant Modulus, TD | 0.175 GPa | 25.4 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® LA-0218-AF LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Base resinFilm properties are typical of blown fi.. |
|||
Secant Modulus, TD | 0.175 GPa | 25.4 ksi | 50 µm (2 mil) film; ASTM D882 |
DuPont Nucrel® 30707 Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating 7 wt% Acrylic Acid.Nucrel® 30707 is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion .. |
|||
Secant Modulus, TD | 0.175 GPa | 25.4 ksi | ASTM D882 |
NOVA Chemicals Novapol® LF-0218-AF LDPE Extrusion Resin
(discontinued **) Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu.. |