Mechanical Properties Metric English Comments
Secant Modulus, TD 0.263 GPa
38.1 ksi
ASTM D882
ExxonMobil Escorene® LD-316 EVA Film Resin, High Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 1.9% vinyl acetate copolymer, high clarity film resin. Film made from LD-316 offers improved impact strength and heat sealability versus homopoly..