Mechanical Properties Metric English Comments
Secant Modulus, TD 0.310 GPa
45.0 ksi
ASTM D882
Chevron Phillips 7109CLT LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene Copolymer, High Slip, Very High Antiblock Version of 7109T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended wit..
Secant Modulus, TD 0.310 GPa
45.0 ksi
ASTM D882
Chevron Phillips 7109DT LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene Copolymer, No Slip, No Antiblock Version of 7109T with Process Aid, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or ble..
Secant Modulus, TD 0.310 GPa
45.0 ksi
ASTM D882
Chevron Phillips 7109LT LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene Copolymer, High Antiblock Version of 7109TCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPEApplications:Ind..
Secant Modulus, TD 0.310 GPa
45.0 ksi
ASTM D882
Chevron Phillips 7109T LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industrial Liners, Stretch Wrap, Garment Bags..
Secant Modulus, TD 0.310 GPa
45.0 ksi
ASTM D882
NOVA Chemicals Sclair® 14K1 Octene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer.
Secant Modulus, TD 0.310 GPa
45.0 ksi
ASTM D882
NOVA Chemicals Sclair® 14K3 Octene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer.
Secant Modulus, TD 0.310 GPa
45.0 ksi
ASTM D882-A
Borealis Borstar® FB4250T LLDPE for Blown Film
Borstar FB4250 is well suited for a wide range of film applications due to its properties. The well balanced mechanical properties will improve the functionality of the films or allow for material ..
Secant Modulus, TD 0.310 - 0.520 GPa
45.0 - 75.4 ksi
Average value: 0.417 GPa Grade Count:15
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and..
Copyright © lookpolymers.com All Rights Reserved