Secant Modulus, TD 0.340 GPa
49.3 ksi
ASTM D882
Huntsman Rexell® M3105 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low medium density copolymer, cast film extrusion, FDA compliantFeatures: Excellent combination of toughness, stiffness, and water vapor barrier with good temperature resistance.Applications:..
Secant Modulus, TD 0.340 GPa
49.3 ksi
ASTM D882
Huntsman Rexell® M3107 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low medium density copolymer, cast film extrusion, FDA compliantFeatures: Excellent combination of stiffness, heat resistance, and impermeability to water vapor.Applications: Food packaging, ..