Secant Modulus, TD 0.0430 - 0.125 GPa
6.24 - 18.1 ksi
Average value: 0.0708 GPa Grade Count:6
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported..
Secant Modulus, TD 0.0430 GPa
6.24 ksi
50 µm (2 mil) film; ASTM D882
DuPont Elvax® 3170 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
18 wt% Vinyl Acetate.Elvax® 3170 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins..