Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.0500 - 1.70 GPa | 7.25 - 247 ksi | Average value: 1.00 GPa Grade Count:85 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Secant Modulus, TD | 0.0500 GPa | 7.25 ksi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ F15 High Density Polyethylene Film Key Characteristics:High productivityHigh tensile strengthHigh dart impactHigh stiffnessLow gel contentGood moisture barrierExcellent printabilityRecommended Applications:High speed processingWide l.. |
|||
Secant Modulus, TD | 0.0500 - 0.241 GPa | 7.25 - 34.9 ksi | Average value: 0.113 GPa Grade Count:8 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |