Mechanical Properties Metric English Comments
Secant Modulus, TD 0.5309 GPa
77.00 ksi
2% Secant; ASTM D882
Dow Saran® 28 Clear Plastic Barrier Film
Saran™ 28 is a clear biaxially oriented monolayer barrier film, designed for chub packaging machines and laminations. It is available in 100 gauge, as single or double wound rolls.Information prov..