Polymer Property : Secant Modulus, TD = 95.7 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.660 GPa
95.7 ksi
ASTM D882
Chevron Phillips HiD® 9647T HDPE Blown Film Resin  (discontinued **)
Resin Type: Linear Polyethylene CopolymerCharacteristics: Copolymerization Enhances Film Toughness, Unique Combination of Density and Melt Index, Excellent Strength Properties as well as Good Heat S..