Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 102 °C
216 °F
Eastman
Westlake Hifor SC74561-F Clear (Voridian) Polyethylene Film, Using Energx Technology Services  (discontinued *
VORIDIAN HIFOR CLEAR SC74558-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and low antiblock additives. Films produced with t..
Heat Seal Strength Initiation Temperature 102 °C
216 °F
ASTM F882
Chevron Phillips MarFlex® D139DK Metallocene Linear Low Density Polyethylene, Blown Film
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du..
Heat Seal Strength Initiation Temperature 102 °C
216 °F
ASTM F882
Chevron Phillips MarFlex® D139FK Metallocene Linear Low Density Polyethylene, Blown Film
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du..
Heat Seal Strength Initiation Temperature 102 °C
216 °F
200 g/in seal strength is achieved
Westlake Hifor SC74560-F Clear Polyethylene  (discontinued **)
Hifor Clear Polyethylene SC74560-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and medium antiblock additives. Films produc..