Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 72.0 °C
162 °F
NOVA Chemicals Sclair® FP112-A Octene VLDPE Film Resin
Features: Low seal initiation temperatureHigh toughnessVery good optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Low gel Applications: Sealant and lamination film for food packagi..