Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 106 °C
223 °F
30 micron
LyondellBasell Adsylâ„¢ 5 C 37 F Polyolefin
Description: Adsylâ„¢ 5 C 37 F is a new thermoplastic polyolefin which has been designed as a BOPP sealing layer material with exceptionally low sealing temperature. It features a high clarity an..
Heat Seal Strength Initiation Temperature 106 °C
223 °F
30 micron
LyondellBasell Adsylâ„¢ 5 C 39 F Polyolefin
Description: Adsylâ„¢ 5 C 39 F is a new thermoplastic polyolefin which has been designed as a BOPP sealing layer material with exceptionally low sealing temperature. It features a high clarity an..
Heat Seal Strength Initiation Temperature 106 °C
223 °F
30 micron
LyondellBasell Adsylâ„¢ 5 X 37 F Polyolefin
Description: Adsylâ„¢ 5 X 37 F is a new thermoplastic polyolefin which has been designed as a BOPP sealing layer material with exceptionally low sealing temperature. It features a relatively high..
Heat Seal Strength Initiation Temperature 106 °C
223 °F
2 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Dow ELITE™ 5100G Enhanced Polyethylene Resin
™ 5100G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers excellent impact strength, good tensile and puncture properties for thick and thin gauge industrial and consume..